HIGH STRENGTH-GEOPOLYMER BUILDING MATERIAL
DOI:
https://doi.org/10.29081/jesr.v28i4.012Keywords:
geopolymer, fly ash, recycled concrete waste, alkaline activator, polymerization reaction, compressive strength.Abstract
New geopolymer concrete with high mechanical strength - 58.9 MPa after 28 days of curing - was experimentally made under environmental friendly and economic conditions. The high-strength-geopolymer is baed on coal fly ash and building concrete waste as geopolymer materials suitable for completely substituting the cement in concrete structure. The alumino-silicate geopolymer materials with binder role were activated in liquid alkaline medium (sodium silicate and sodium hydroxide) for facilitating the polymerization reaction that turns the alumino-silicate wastes into geopolymer concrete. The use for the first time in this experiment of recycled building concrete waste from demolition is the work originality.
Downloads
Download data is not yet available.
Downloads
Published
2023-02-09
Issue
Section
Articles
How to Cite
HIGH STRENGTH-GEOPOLYMER BUILDING MATERIAL. (2023). Journal of Engineering Studies and Research, 28(4), 107-115. https://doi.org/10.29081/jesr.v28i4.012